SAE AMS7000 Revision A

Original price was: $70.00.Current price is: $42.00.

Laser-Powder Bed Fusion (L-PBF) Produced Parts, Nickel Alloy, Corrosion- and Heat-Resistant, 62Ni – 21.5Cr – 9.0Mo – 3.65Nb Stress Relieved, Hot Isostatic Pressed and Solution Annealed

standard by SAE International, 05/16/2022

This Document Only Available In PDF.

Category:

SAE AMS7000A – Laser-Powder Bed Fusion (L-PBF) Produced Parts, Nickel Alloy, Corrosion- and Heat-Resistant, 62Ni – 21.5Cr – 9.0Mo – 3.65Nb Stress Relieved, Hot Isostatic Pressed and Solution Annealed

This specification covers a corrosion and heat-resistant nickel alloy in the form of parts produced by laser-powder bed fusion (L-PBF) that are subjected to post-deposition stress relief (SR), hot isostatic press (HIP) and solution anneal operations. Parts may require subsequent machining or surface finishing to meet specific application requirements.

Product Details

Published:
05/16/2022
File Size:
1 file , 250 KB
Note:
This product is unavailable in Ukraine, Russia, Belarus